TITANEX® HP0891B High density polyethylene resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: HP0891B is a compound high density polyethylene for pipe application meeting ISO/TR for PE80 classification.Applications: Water pipe, municipal pipe, industrial pipe. Advantages: Outstanding stress crack resistance, high hoop stress, low temperature toughness, high strength. Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- ESCR 100% Igepal®
- Oxidative Induction Time (OIT)
- Carbon Black Loading
- Base Resin Melt Index
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- 1% Secant Modulus
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
- Cooling Water Temperature
- Minimum Required Strength (MRS) Mpa
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|