TITANLENE® LDC800YY Low density polyethylene resin
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: Low density polyethylene for extrusion coating.Applications: Coating for all substrates Additives: Barefoot Advantages: - Good drawdown
- Good heat seal ability and adhesion properties
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Vapor Transmission
- Oxygen Transmission
- Base Resin Melt Index
- Neck In
- Vicat Softening Point
- Processing Temperature
|
|
|
|