Techmer Lehvoss Compounds Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone
Subcategory: Polycarbonate; Thermoplastic; Polymer
Material Notes: Information provided by TL Compounds.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|