Techmer Lehvoss Compounds Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Cvarbon Filled
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Conductive Carbon, Powder Modified Information provided by Techmer Lehvoss Compounds.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Surface Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |