Techmer Lehvoss Compounds Luvotech™ J-54/10 Polycarbonate, 10% GFR
Subcategory: Polycarbonate; Thermoplastic; Polymer
Material Notes: Polycarbonate is one of the toughest and most versatile of all engineering thermoplastics. The combination of glass and flame-retardants provides additional features to allow for enhanced design capabilities. These products offer the excellent dimensional stability and toughness normally associated with polycarbonate, as well as increased stiffness and heat resistance. Information provided by TL Compounds.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|