Techmer Lehvoss Compounds Plaslube® NY-1/TF/10 Nylon 66, 10% PTFE
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66
Material Notes: Plaslube polytetrafluroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearings and bushings. Information provided by TL Compounds.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Coefficient of Friction
- Coefficient of Friction, Static
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|