Solvay Solexis Tecnoflon® N 605K Copolymer Fluoroelastomer, Non-curative
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Superior metal-to-rubber bonding along with excellent hot tear resistance. 65% fluorine. Superior for: Injection/Compression Molding; Compression Molding; Shaft Seals; Valve Stem Seats; Molded Goods; Bonded Articles; Complex Shapes Data provided by the manufacturer Solvay Solexis, Inc.
| Available Properties |
- Mooney Viscosity
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Compression Set, Elevated Temperature
|
|
|
|