Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Key Words: TPUR; Toyobo Company
Material Notes: Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc. Information provided by Toyobo Co., Ltd
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|