Toyobo T-602G30 Aromatic Nylon, 30% Glass Reinforced (DAM)
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Features: 30% Glass Fiber Reinforced, Good Appearance Information provided by Toyobo.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Volume Resistivity
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|