Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant
Subcategory: Polycarbonate; Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Applications: - Lamp parts
- Home electric appliance parts
Features: - Fine appearance
- High rigidity
- Impact resistant
Information provided by Toyobo.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|