Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Material Notes: Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General Purpose Applications: - Automobile engine head covers
- Hot plates
- Vending machine parts
- Umbrella ribs
Information provided by Toyobo.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|