TPUCO UR50 Polyester Urethane Rubber
Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset
Material Notes: UR50 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of conventional rubber manufacturing equipment and techniques to yield finished urethane parts. Compounds of urethane rubber can be molded by compression, injection, and transfer molding procedures. Excellent mold definition is obtainable in press cures. The linear shrinkage of vulcanizates of UR varies somewhat with the type of loading, but, in general this value is approximately 1.5%, which is comparable to that of neoprene. Excellent mold release is provided by lubricant of M-7 or silicone mold release lubricants, but indiscriminate use can cause poor flow and knitting problems. Information provided by Taiwan PU Corporation.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 300% Modulus
- Tear Strength
- Compression Set
- Processing Temperature
- Cure Time
- Color
- Health Hazard
- Odor
- Physical Form
- Storage Stability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|