TPUCO PTMG CPU-167L Polyurethane Casting Elastomer
Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset
Material Notes: A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing. Information provided by Taiwan PU Corporation.