TPUCO TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer
Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset
Material Notes: 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It has excellent physical properties, chemical resistance, and abrasion resistance. Applications: - Protective coating
- Abrasion resistant coating
- Pipe coating
- Flooring
- Roof and deck coating
- Construction coating
- Industrial coating
- Low cost molds
- Spray-mold type
- Highway and bridge overlays
- Watertight coating
- Roller, other casting elastomer replacement
- Foam surface protection
Information provided by Taiwan PU Corporation.
| Available Properties |
- Density
- Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Processing Temperature
- Mixing Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|