American Balsa Wood
Subcategory: Wood; Hardwood
Key Words: Ochroma pyramidale; Lumber, Timber
Material Notes: High buoyancy value, and good insulating value Usual surface texture: Fine Dimensional changes when dried lumber is subjected to variations in humidity during service: Small Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years) Resistance to penetration by preservatives: Resistant Common Applications: Useful for heat sound and vibration insulation. Buoyancy aids
| Available Properties |
- Density
- Poissons Ratio
- Machinability
- Color
|
|
|
|