American Maple, Rock (Sugar Maple)
Subcategory: Wood; Hardwood
Key Words: Acer saccharum; Lumber, Timber
Material Notes: High resistance to abrasion. Diffuse-Porous Hardwood. Least easy to work with hand tools. Excellent shaping, fair planing, fair steam bending. Data is based on small, clear, air-dried samples unless specified. Usual surface texture: Fine Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years) Resistance to penetration by preservatives: Resistant Common Applications: Excellent flooring timber. Furniture. Sports goods Property values marked by an asterisk (*) have been taken from an unusually old reference source.
| Available Properties |
- Density
- Density
- Cell Length
- Hardness, Wood Indentation
- Tensile Strength, Ultimate
- Modulus of Rupture
- Modulus of Rupture
- Flexural Modulus
- Flexural Modulus
- Flexural Yield Strength
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Yield Strength
- Poissons Ratio
- Machinability
- Shear Strength
- Shear Strength
- Impact
- Work to Elastic Limit
- Work to Maximum Load
- Toughness
- Cleavage
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|