European Redwood Wood
Subcategory: Wood; Softwood
Key Words: Pinus sylvestris; Lumber, Timber
Material Notes: Usual surface texture: Medium Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years) Resistance to penetration by preservatives: Moderately resistant Common Applications: Construction, joinery, furniture
| Available Properties |
- Density
- Machinability
- Color
|
|
|
|
| Property Data |