Afrormosia Wood
Subcategory: Wood; Hardwood
Key Words: Pericopsis elata; Lumber, Timber
Material Notes: Tends to darken on exposure, stains in contact with iron in damp conditions. Usual surface texture: Medium/fine Dimensional changes when dried lumber is subjected to variations in humidity during service: Small Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years) Resistance to penetration by preservatives: Extremely resistant Common Applications: Interior and exterior joinery. Furniture. Cladding.
| Available Properties |
- Density
- Water Absorption
- Machinability
- Color
|
|
|
|