Pitch Pine Wood
Subcategory: Wood; Softwood
Key Words: Pinus palustris, Pinus Elliottii, Pinus Resinosa; Red Pine, Lumber, Timber
Material Notes: Also known as longleaf yellow pine or longleaf pitch pine or American pitch pine. Test material of southern USA origin. Usual surface texture: Medium Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Moderately Durable (10 to 15 years) Resistance to penetration by preservatives: Resistant Common Applications: Interior and exterior joinery, heavy construction
| Available Properties |
- Density
- Water Absorption
- Poissons Ratio
- Machinability
- Color
|
|
|
|
| Property Data |