South American Parana Pine Wood
Subcategory: Wood; Softwood
Key Words: Araucaria Angustifolia; Lumber, Timber
Material Notes: Distortion may occur in drying Usual surface texture: Fine Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years) Resistance to penetration by preservatives: Moderately Resistant Common Applications: Interior joinery. Plywood