Plywood
Subcategory: Wood
Key Words: Timber, Lumber
Material Notes: Plywood is made of several thins layers, or 'plies' that are laminated together. The layer structure leads to more uniform properties than solid wood, since the effects of grain anisotropy are minimized. The properties of plywood vary with the quality of the constituent layers; typical values are listed below.
| Available Properties |
- Tensile Strength, Ultimate
- Flexural Modulus
- Compressive Yield Strength
- Shear Modulus
- Shear Strength
- CTE, linear 20°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|