Tropical Idigbo Wood
Subcategory: Wood; Hardwood
Key Words: Terminalia Ivorensis; Lumber, Timber
Material Notes: Stains yellow in contact with water, is acidic and may corrode ferrous metals, also stains in contact with iron when wet Data is based on small, clear, air-dried samples unless specified. Usual surface texture: Medium Dimensional changes when dried lumber is subjected to variations in humidity during service: Small Resistance to fungal decay (Heartwood in ground contact): Durable (15 to 25 years) Resistance to penetration by preservatives: Extremely resistant Common Applications: Interior and exterior joinery, plywood
| Available Properties |
- Density
- Hardness, Wood Indentation
- Tensile Strength, Ultimate
- Modulus of Rupture
- Flexural Modulus
- Compressive Yield Strength
- Machinability
- Shear Strength
- Toughness
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|