Fir, Subalpine
Subcategory: Wood; Softwood
Key Words: Abies Lasiocarpa, Lumber, Timber
Material Notes: These firs are sold as white firs in the U.S., they hail from California, Oregon, Washington, western Montana, and northern Idaho.
| Available Properties |
- Specific Gravity
- Hardness, Wood Indentation
- Modulus of Elasticity
- Modulus of Rupture
- Compressive Strength
- Poissons Ratio
- Shear Strength
|
|
|
|