Collagen
Material Notes: Collagen is a family of proteins with multiple structural characteristics and multiple functions in the human body. It has mechanical uses in bone, skin, tendon, and ligament and also biological functions such as controlling gene expressions in development.
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
|
|
|
|
| Property Data |