UBE F222Polyethylene
Subcategory: Polyethylene; Thermoplastic
Material Notes: Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical properties including transparency and glossiness, and making the material ideal for further processing. Transparency:Superior transparency and glossiness even for applications involving processing of thick objects. Ease of Processing: Excellent fluidity and melt tension characteristics suited to a wide range of molding methods. - Inflation molding - can be molded into even thick or wide products with superior bubble stability.
- Extrusion lamination - can be drawn down even at high speed.
- Blow molding - can be molded producing a very smooth surface.
- Injection molding - can be molded even into very thin products.
Strength: Good balance in length and breadth with superior tearing strength lengthways. Application: General packing Features: Moldability Transparency Glossiness Information provided by UBE.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Strength
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|