UBE 1024FD-1 Nylon 6 Film
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: T-die cast film of 25µm in thickness Information provided by UBE.
| Available Properties |
- Oxygen Transmission Rate
- Thickness
|
|
|
|