UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.8)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Specialties: Monomer containing type of 1022T Applications: Fishing net, Small size monofilament, Softness required applications Information provided by UBE.