UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter = 2 mm)
Subcategory: Nylon; Thermoplastic; Nylon 612
Material Notes: Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the water Applications: Small- large size sport fishing line and long line (branch line), Appearance of filament is said to be "brilliant crystal tone" and reputed in the branch line application Information provided by UBE.