UBE P7115U Electronic Grade Nylon Copolymer Powder
Subcategory: Nylon; Thermoplastic; Nylon 612
Material Notes: Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication Systems through the world. Comments: nylon 6/12 copolymer Information provided by UBE.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|