UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron and steel gas mains. The excellent performance, especially creep and chemical resistance UBESTA supports industry as one of the most reliable materials. Comments: heat resistance, black color Information provided by UBE.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
- Feed Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Die Temperature
- Mold Temperature
- Roll Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Hold Pressure
- Back Pressure
- Screw Speed
- C/R
- Calibrating Vacuum
- Calibration
- Compression Ratio
- Die Diameter
- Die Gap
- Die Width
- Extruder
- Extruder Characteristics
- Film Thickness
- Flight Depth in the Feeding Zone
- Flight Depth in the Metering Zone
- Haul Off Speed
- Haul Speed
- Injection Speed
- L/D Ratio
- Length of Compression Zone
- Length of Feeding Zone
- Length of Metering Zone
- Mandrel Diameter
- Peripheral Screw Speed
- Water Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|