UBE UBEPOL-VCR303 New Type Synthetic Rubber (Raw Polymer)
Subcategory: Elastomer, TS; Thermoset
Material Notes: Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high melting point and crystallinity, and high cis-1,4-polybutadiene rubber matrix. UBEPOL-VCR is improved on the processability and a lot of physical properties of the conventional polybutadiene rubber (BR). Information provided by UBE.
| Available Properties |
- Density
- Volatiles
- Mooney Viscosity
- Ash
- n-Hexane Insolubles (weight %)
|
|
|
|