UBE UBEPOL-BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Subcategory: Elastomer, TS; Thermoset
Material Notes: Description: UBEPOL BR is UBE's line of polybutadiene rubber products. Information provided by UBE.
| Available Properties |
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 200% Modulus
- 300% Modulus
- Rebound
- Tear Strength
- Abrasion
- Compression Set
- Cut Generation De Mattia Flexing Machine
- Cut Growth (2mm-->15mm) De Mattia Flexing Machine
- Goodrich Flex, 0.175" Stroke, 55lb, 100°C, P.S.
- Wet Skid Resistance on Safety-Walk
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|