UBE UPIMOL-S High Heat Polyimide Shape

 

Subcategory: Polyimide, TS; Thermoset

Material Notes:
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ube, produced through polycondensation of biphenyltetracarboxylic dianhydride and diamine. Depending on the type of application, there are two types of UPIMOL available. One is UPIMOL-R for general use and the other is UPIMOL-S for high heat-resistant use.

While exhibiting a number of excellent properties over a wide temperature range, of special note are UPIMOL's exceptional mechanical, thermal and chemical properties at high temperatures. Since UPIMOL has been shown to satisfy even the exacting requirements of the ceramics industry, its applications are extremely wide-ranging, the major uses including:

  • Electrical and Electronic Equipment
    • IC sockets for semiconductor testing machine handlers
    • Collet for IC mounter
    • Frictional parts such as copier bearings
    • Wire guides for wire dot printers
  • Industrial Equipment
    • Piston rings for compressors, etc.
    • Thrust washers for gears, etc.
    • Radiation and chemical resistant pipe sealings and other such parts.
  • Aerospace-Related Equipment
    • Vane bushings for jet engines
    • Spline couplings for aircraft
    • Insulating parts, spacers, etc, for artificial satellites.

Information provided by UBE.

Available Properties
  • Water Absorption
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Strength
  • Compressive Modulus
  • Izod Impact, Notched
  • Izod Impact, Unnotched
  • Coefficient of Friction
  • Limiting Pressure Velocity
  • Abrasion
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Decomposition Temperature
  • Compressive Creep
  • Thermal Weight Reduction (in Air)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。