UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape
Subcategory: Polyimide, TS; Thermoset
Material Notes: Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durability for oxygen plasma, vacuum degassing properties, low water absorption and good processability. Heat distortion temperature is 470°C. Applications: - Semiconductor production equipment parts
- Vacuum equipment parts
- Precisely processed parts
- Heat and chemical resistant gaskets and sealing materials
Features: - Super high heat resistance (Heat distortion temperature: 470°C)
- Excellent plasma resistance
- Low out gas
- Good processability
- Very low impurities
- Low water absorption
Information provided by UBE.
| Available Properties |
- Specific Gravity
- Water Absorption
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Flexural Modulus
- Flexural Strength
- Limiting Pressure Velocity
- Taber Abrasion, mg/1000 Cycles
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 250°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Decomposition Temperature
- Durability for O2 Plasma
- Vacuum Degassing
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|