Valley Adhesives EM-110 High Performance Application Glue Stick
Subcategory: Adhesive; Thermoset
Material Notes: Valley Adhesives EM-110 High Performance Application Glue Stick High peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, polyolefins, metal, foam, textiles, and non-wovens.
| Available Properties |
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Peel Strength
- Maximum Service Temperature, Air
- Softening Point
- Pot Life
- Color
|
|
|
|