Valley Adhesives EM-120 High Performance Application Glue Stick
Subcategory: Adhesive; Thermoset
Material Notes: Valley Adhesives EM-120 High Performance Application Glue Stick General purpose hot melt spray adhesive; High performance and heat resistance with excellent adhesion, shear, peel and high initial strength; High adhesion bonding on most substrates including open cell foam and polyolefins.
| Available Properties |
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Peel Strength
- Maximum Service Temperature, Air
- Softening Point
- Pot Life
- Color
|
|
|
|
| Property Data |