PolyOne Geon® 78702 Interior Extrusion PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Superior ductilityData provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|