PolyOne Geon® 78714 Pipe PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: High Impact. Type II, Grade 1, low shear cube compound for pipe and conduit extrusion.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|