PolyOne Geon® 83530 Fiberloc PVC; 30% Glass Fiber Reinforced
Subcategory: Vinyl; Thermoplastic; Polymer
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Medium Impact, High Flow. Weatherable, high flow, 30% glass fiber reinforced compound for injection molding or extrusion applications.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Izod Impact, Notched
- Izod Impact, Unnotched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|