PolyOne Geon® 87319 Molding PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: High Flow, High Impact, Transparent, Interior.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Flammability, UL94
- Haze
- Transmission, Visible
- Processing Temperature
|
|
|
|