PolyOne Geon® 87761 Powder PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Interior grade, rigid PVC powder compound designed for high speed extrusion of vertical blinds on multi-screw extruders having high or ultra-high shear screws.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|