PolyOne Geon® M2115 Molding PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Normal Flow, High Impact, Transparent, Interior. A unique packaging material providing the look of frosted glass using conventional vinyl tooling. Containers produced using this material exhibit high impact resistance with excellent chemical resistance.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|