PolyOne Geon® M2150 Molding PVC; Opaque Grade
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Normal Flow, High Impact, Opaque, Interior. Translucent, general purpose extrusion blow molding compound. Designed to be used with pigmentation for opaque bottle applications. Exhibits superior gloss. Is compounded to extrude at rates 10-15% faster thData provided by the manufacturer, The Geon Company.