PolyOne Geon® W1203 Wire & Cable PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Premium grade building wire insulation. UL83 bulletinized for THHN,THWN, THW, TW and 105°C AWM. THW2, THN2, Apparatus Wire Style Number 1005, 1006, 1010 (CSA TR 64).Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Surface Resistance
- Brittleness Temperature
- Oxygen Index
- Processing Temperature
|
|
|
|