PolyOne Geon® W2410 Wire & Cable PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Flame retardant 60°C rated sunlight resistant for indoor/outdoor distribution.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Brittleness Temperature
- Oxygen Index
|
|
|
|