PolyOne Geon® W3204 Wire & Cable PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Geon W3204 is a tough semi-rigid PVC compound intended for UL Subject 758, Style 1061 and Canadian Standards Association Type SR.Data provided by the manufacturer, The Geon Company.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Brittleness Temperature
- Oxygen Index
- Processing Temperature
|
|
|
|