VTC Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mechanical properties, such as elongation, compression set, tensile and tear strength. The low density entails lower weight compared to the 600 and 660-series. Information from Vita Thermoplastic Polymers (VTP).
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Bonding to PP
- Chemical Resistance
- Color
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|