VTC Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine the advantages of the other two series. The material has good flow and mechanical properties as well as reasonable scratch resistance. Information from Vita Thermoplastic Polymers (VTP).
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Bonding to PP
- Chemical Resistance
- Color
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|