VTC Mediprene™ 500600M TPE, Medical Applications, 60A Hardness
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:- Low extractable
- No migration of plasticizer
- Cleanliness
- Good vapor and gas transmission properties
- Softness, flexibility and clarity
- Chemical inertness
- Ease of sterilization for repeated use
Mediprene™ compounds can be processed using conventional thermoplastic equipment for extrusion, injection molding, etc. The compounds are not hygroscopic, and thus do not need any pre-drying. Assembling Mediprene™ to mainly all used thermoplastics is feasible. All Mediprene™ grades are fully recyclable and where possible reprocessable during manufacturing and when burned do not emit toxic fumes. Mediprene™ grades exhibit excellent resistance to many fluids used in the healthcare environment. Information from Vita Thermoplastic Polymers (VTP).
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Chemical Resistance
- Color
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|