|   VTC Mediprene™ 500750M TPE, Medical Applications, 75A Hardness  Subcategory: Elastomer, TPE; Thermoplastic Material Notes: All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications.  In both medical and food contact areas, high application demands are found, such as:
 Low extractableNo migration of plasticizerCleanlinessGood vapor and gas transmission propertiesSoftness, flexibility and clarityChemical inertnessEase of sterilization for repeated use
 Mediprene™ compounds can be processed using conventional thermoplastic equipment for extrusion, injection molding, etc.  The compounds are not hygroscopic, and thus do not need any pre-drying.  Assembling Mediprene™ to mainly all used thermoplastics is feasible. All Mediprene™ grades are fully recyclable and where possible reprocessable during manufacturing and when burned do not emit toxic fumes. Mediprene™ grades exhibit excellent resistance to many fluids used in the healthcare environment. Information from Vita Thermoplastic Polymers (VTP). 
| | 
    | Available Properties |  
    | Specific GravityMelt FlowHardness, Shore ATensile Strength at BreakElongation at Break100% Modulus300% ModulusTear StrengthMaximum Service Temperature, AirMinimum Service Temperature, AirProcessing TemperatureChemical ResistanceColorWeather Resistance
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |